Sarfaraz Moh
The color of poly or amorphous silicon deposited PECVD
Sarfaraz Moh
2004-09-02
Dear Jinkee

The colour might be due to the thickness as there is
N2 in the chamber there might be N2 in the film.

Why dont you analyse the film using Ellipsometry,
SEM-EDS or XPS. If you have the facility.

Thanks
Sarfaraz Moh
Thin film centre
University of Paisley
UK





___________________________________________________________ALL-NEW Yahoo!
Messenger - all new features - even more fun!  http://uk.messenger.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group