Ti Waveguides in Lithium Niobate
2004-09-01
Jeffrey Price
2004-09-02
Brent Garber (2 parts)
2004-09-03
Bruno Wacogne
2004-09-02
Gary
Ti Waveguides in Lithium Niobate
Bruno Wacogne
2004-09-03
Hi Jeff,

How thick are your Ti strips ? If it is too thin it may look completely
diluted in the crystal.

Regards,

Bruno Wacogne


At 15:03 01/09/2004 -0400, you wrote:
>Hello,
>
>I am trying to diffuse Ti strips into Lithium Niobate.  The strips run
>from approximately 3 -10 um.  After diffusion (which I have run
>different permutations ranging from 1-9h and 900-1050C) in a wet
>nitrogen environment the waveguides completely disappear.  I know that
>the index delta should be approximately .01 so they should be difficult
>to see, but I can't seem to see anything at all.  I was wondering if
>anyone has had this problem before or can help me find a solution.  Thanks.
>
>Jeff Price
>Research Assistant, University of Delaware
>[email protected]
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/
>
***********************************************
*                                             *
*   Bruno Wacogne                             *
*   Laboratoire d'Optique P.M. Duffieux       *
*   Faculté des Sciences et des Techniques    *
*   Route de Gray                             *
*   25030 Besançon cedex                      *
*                                             *
*   tel  (++33) 3 81 66 64 25                 *
*   fax  (++33) 3 81 66 64 23                 *
*   mel  [email protected]         *
*                                             *
* http://imfc.univ-fcomte.fr/lopmd/index.html *
* http://imfc.univ-fcomte.fr/                 *
*                                             *
***********************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMS Technology Review
Mentor Graphics Corporation