Removing sawing residues from Si surface
2004-09-02
Karin Buchholz
2004-09-02
Kenneth Smith
2004-09-03
newman
2004-09-02
Kasman , Elina
2004-09-03
Dekker, R. (Ronald)
Removing sawing residues from Si surface
newman
2004-09-03
Hi Karin
              Did you let the wafer surface dry after cutting ?
This is a definite MUST NOT DO.
Once surface is dry the thin oxide layer forming on the particles sticks
them firmly to the wafer surface.
Keep the wafers wet then transfer them to a very dilute surfactant (Soap
solution) this with ultrasonics should do the trick.
Then wash again in DI.

Alternatively talk to EVG EVGroup.com who make a megasonic wafer cleaner
to do the trick.

Best regards

Jan Newman  (EVG, UK and Ireland)





>Dear all,
>
>I cut a fresh wafer into pieces using a diamond wafer saw and distilled
>water. However I did not cover the surface to protect it from dirt.
>
>What is the best way to remove the residues from the Si surface without
>roughening it? For the application of biological layers I need really
>smooth surfaces.
>
>Right now I am trying DI water in an ultrasonic bath, but this seems
>not efficient enough...
>
>Any helpful tips are greatly appreciated!
>
>Thank you, Karin
>
>--  Walter Schottky Institut
>Technische Universitaet Muenchen
>
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/

--
newman

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Addison Engineering