A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Maximum current density for Au
Maximum current density for Au
2004-09-07
Kasman , Elina
Maximum current density for Au
Kasman , Elina
2004-09-07
I have been unable to find information on how to calculate the maximum
current density for gold conductors in the circuit.
We have 500nm thick gold evaporated onto glass substrate (Pyrex, with Cu
adhesion layer).

Does anyone have experimental data on maximum allowable current?

Thanks
Elina