MEMSnet Home: MEMS-Talk: silicon oxide properties
silicon oxide properties
2004-09-15
Mihaela Miu
2004-09-15
Venkatachalam Chokkalingam
2004-09-15
Paul French (2 parts)
intellisuite software
2004-09-24
piyush tilloo
2004-09-25
koshy
query regarding simulation of design
2004-09-26
piyush tilloo
silicon oxide properties
Paul French
2004-09-15
Hi Miheala,

This article may help, it a how to calculate Si modulus Young's modulus,
Poisson ratio, etc. I think I originally got it from someone on this MEMs
discussion list.. If its not what you're looking for, it at least has
references that do provide a 'how to calculate' these things.

Cheers,

Paul






-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Mihaela Miu
Sent: 15 September 2004 13:57
To: [email protected]
Subject: [mems-talk] silicon oxide properties

Hi All;


Does anyone know about silicon oxide properties like density, Young's modul,
Poisson ratio, or conductivity?
Where can I get this information?

Regards;

Mihaela

Mihaela Miu
National Institute for Research and Development in Microtechnologies
(IMT - Bucharest)
Erou Iancu Nicolae 32B, 72996 Bucharest, Romania
http://www.imt.ro 
Phone: +40-21-490.84.12;
Fax: +40-21-490.82.38

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
elasticity_tutorial (2).pdf (application/pdf, 422892 bytes)
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
University Wafer
Nano-Master, Inc.