All-

Have a problem with BPSG deprate. We have tried every logical thing
possible on the tool. As far as dopant don't flow, the films behave
same between the good and bad tool. Also all other films run fine on
the bad tool. Individual incorporation of B2H6 or PH3 or both show
10% deprate differnces between the good tools and the bad. Any
suggestions?

Sathya.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation