Brijesh Raut
2004-09-28
Brubaker Chad
wafer level packaging
Brubaker Chad
2004-09-28
Brijesh,

It depends on what kind of information you are looking for in WLP.  Its actually
a pretty large field, and can include processes for wafer bumping and flip chip
packaging (where the primary processes are lithographic and plating) to full
wafer level bonding.

A reference listed previously in this forum has some good basic information on
wafer level bonding:

Fundamentals of Microfabrication
by Marc Madou



Best Regards,
Chad Brubaker

EV Group       invent * innovate * implement
Technology - Tel:  480.727.9635, Fax:  480.727.9700  e-mail:
[email protected], www.EVGroup.com

This message and any attachments contain confidential or privileged information,
which is intended for the named addressee(s) only. If you have received it in
error, please notify the sender immediately and then delete this e-mail. Please
note that unauthorized review, copying, disclosing, distributing or otherwise
making use of the information is strictly prohibited.

 -----Original Message-----
From:   [email protected] [mailto:[email protected]]  On
Behalf Of Brijesh Raut
Sent:   Tuesday, September 28, 2004 9:56 AM
To:     'General MEMS discussion'
Subject:        [mems-talk] wafer level packaging



hi everybody,

I am very new to wafer level packaging(WLP) and wafer bonding in MEMS
technology, so can any one assist me to find the basic concept and ideas for
WLP.

sincerely
brijesh


-------------------------------------------------
This mail sent through IMP: http://horde.org/imp/

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
University Wafer
The Branford Group