MEMSnet Home: MEMS-Talk: Re: Tantal biocompatibility
Re: Tantal biocompatibility
1998-11-23
Albert K. Henning
Re: Tantal biocompatibility
Albert K. Henning
1998-11-23
Galia Georgieva wrote:
>
> Dear Sirs,
>
> I am a research student at the Technical University at Dresden,
> Germany. I work on a project about Ta-based films for biocompatible
> microsystems. Could you please tell me whether Ta (and its derivates)
> really is biocompatible? Where could I find information? Or do you
> have any other suggestions? Thank you very much for your help,
>
> yours sincerely,
>
> Galia
>
Check with Prof. Greg Kovacs at Stanford ([email protected]).
Also, Prof. Ken Wise at the University of Michigan may have some
knowledge of this issue.

Al
--
Albert K. Henning, Ph.D.    650/617-0854 (Office)
Redwood Microsystems        650/326-9217 (FAX)
1020 Hamilton Avenue        [email protected]
Menlo Park, CA  94025       http://www.redwoodmicro.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation