MEMSnet Home: MEMS-Talk: Su-8 to PMMA selective etch
Su-8 to PMMA selective etch
2004-10-20
Lidija Malic
Su-8 to PMMA selective etch
Lidija Malic
2004-10-20
Hi Everyone,
I am trying to make multimode waveguides using spin-coated PMMA as
cladding and SU-8 as core material. I do not have much experience with
SU-8 and I would like to know if there is a selective etchant that will
not attack the PMMA cladding, while etching the unexposed SU-8 layer. Any
recommendation will be of great help.
Thanks,
Lidia


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Mentor Graphics Corporation
The Branford Group