MEMSnet Home: MEMS-Talk: gold, photoresist, UV light, bubbles
gold, photoresist, UV light, bubbles
2004-11-29
Rick Giuly
2004-11-29
Z.,W.Y.(Lydia)
2004-11-30
Brad Cantos
2004-11-30
Marco Doms
gold, photoresist, UV light, bubbles
Z.,W.Y.(Lydia)
2004-11-29
Rick,

How can you deterimed that it is gas bubbles?

If you use sylgard 184, there are curing-agent particles existing. Those
particles are also transparency!

Good luck,

Lydia


Quoting Rick Giuly :

> Hello All,
>
> Listed from top to bottom, I have these layers:
> 8 micron AZ P4620 photoresist (spun on)
> ..5 micron gold (ebeam at ~10e-6 torr, 5A per sec)
> 10 micron PDMS (spun on)
> glass substrate
>
> When I expose with UV light, gas bubbles form between the gold and the
> PDMS. They do not form if there is no photoresist.
>
> Any ideas on where the bubbles come from and how to get rid of them?
>
>
> -Rick Giuly
>  GA Tech
>
>
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>




-------------------------------------------------
This mail sent through IMP: http://horde.org/imp/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
University Wafer