MEMSnet Home: MEMS-Talk: Bulk Modulus PDMS (in liquid form)
Bulk Modulus PDMS (in liquid form)
2004-12-12
Nathan L. Tyson
2004-12-13
Jeff Zahn
2004-12-13
Wilson, Thomas
Bulk Modulus PDMS (in liquid form)
Nathan L. Tyson
2004-12-12
Dear Sirs,
        I am using Gelest PDMS (trimethylsiloxy terminated) Silicone Oil
(5cSt.)in
my research and have been unsuccessful in locating an estimate (or better
if possible) of the Bulk Modulus of this oil (not crosslinked, but rather
BM of material in liquid form). I assume that this property is temperature
dependent, and if so, could you give me an idea of how radically its value
varies with temperature? I am using it at 20C and so the BM at this temp
would be most useful. Thanks for your time and assistance. I look forward
to your response.
Cheers,
Nathan L. Tyson

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
The Branford Group
Addison Engineering