Plating Au on Ni.
David Nemeth
2005-01-03
The nickel oxidizes on contact with air.  Follow the nickel evaporation with
a gold evaporation (a few hundred angstroms should be fine).  Do not break
vacuum between the depositions.  The gold plating should then work.

David Nemeth
Senior Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
Cell: (202) 288-1067
Ph: (703) 961-9573 x206
Fax:(703) 961-9576

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of
[email protected]
Sent: Monday, January 03, 2005 4:28 AM
To: [email protected]
Subject: [mems-talk] Plating Au on Ni.


Hello,

We are making process where we would like to plate gold features using
thick PR-mold. Process we had in mind was following:

1.    Evaporate Ni layer on GaAs-wafer.
2.    Make thick PR-mold
3.    Plate Au-trough mold on Ni
4.    Remove PR
5.    Etch Ni away using plated Au as a etch mask

However we have problems with plating on Ni. It just is not plating
anything. Should we try to make some pretreatment to Ni before try to plate
Au?

We have fresh and clean chemical with correct pH. Also plating Au on Au is
working correctly. We are making our plating with Enthone Nuronex 309B
plating solution (should be same stuff than Microfab Au150).

Best regards,
Jukka Viheriälä

***********************************************
Jukka Viheriälä, Researcher

Optoelectronics Research Centre
Tampere University of Technology
P.O. Box 692
FIN-333101 Tampere, Finland

Tel.: +050 595 4147
Fax  +358 3 3115 3400
Email: [email protected]



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics