Hello

we want to pattern gold. We want to work on different materials and we want
to transfer the gold from one material to the other.
That is why we need informations of the adhesion of gold to different
materials. Especially a comparison, because we have to use a hierachie of
adhesions; In order to transfer gold from on material to another a
difference in adhesion is necessary.
Is there any referrence or something else where i could find this
informations?

Does anybody know a recipe for electroplating gold onto Silicon?

Thank you

Daniel

****************************************
Dipl.phys Daniel Schwaab

molecular Bioelectronics
Institute for Thin Films and Surfaces
Research Center Jülich GmbH
52425 Jülich
Germany

Tel: 02461-61 2606
Fax           8733

email: d.schwaab@fz-jülich.de
****************************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics