Hi, Heng,

If Sylgard 184 is the PDMS you referred, I do not think it will reach submicron.
The curing agent is round 10um that have been discussed at this group. For my
experience, you will see very rough surface, i.e., lots of dots, when you spin
coating the film thinner than 10 um.

If you active the PDMS surface, e.g. O2 plasma etching, it is very easy to joint
two PDMS layer.

Good luck,

Lydia

Quoting Xin Heng :

> Hi,
>   I have two questions on microfluidic devices. I hope someones here can
> give me some hints. Thanks
>   1) I was thinking of binding a PDMS layer and a PMMA layer by simply
> attaching them together and 80C baking for a couple hours. But there seems
> to be some bubbles always when I tried using electrokinetics to rive the
> flow
>   2) Alternatively I am thinking of attaching two PDMS layers together.
> But in this case, I might require one PDMS layer to be submicron thick,
> say, 300nm. Is this goal achievable with conventional spin coating
> techniques?
>
>
> >               Best Wishes,
>
>                               Xin Heng
>                               Electrical Engineering of Caltech
>                               M/C136-93, 1200 E California Blvd
>                               Pasadena, CA, 91125, U.S.A
>
>                               office(Moore 337):1-626-395-8870
>                               lab(Moore 4):1-626-395-4711
>                                            1-626-395-8953
>                               fax:1-626-395-8952
> ------------------------------------------------------------------------
> 'If I am not in lab, I'm working in office. If I'm not in my office,
> then I'm on my way to it. -- X. H.'
> ------------------------------------------------------------------------
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>

-------------------------------------------------
This mail sent through IMP: http://horde.org/imp/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing