Two metal layer process
2005-01-17
Li Wang
2005-01-18
shay kaplan
2005-01-18
David Nemeth
Re: Two metal layer process
2005-01-18
Li Wang
Two metal layer process
shay kaplan
2005-01-18
Li,
You are probably right about the Al native oxide. Try to sputter etch the
oxide before Cr deposition.
shay

reply