Help: RIE with small feature size
2005-01-25
William Lanford-Crick
Help: RIE with small feature size
William Lanford-Crick
2005-01-25
Hi,
I don't have any experience with Silicon etching, but a SiO2
mask will be etched quite fast by an SF6-based plasma....A
photoresist mask might work well (in Bosch process) or you
could try a lift-off metal mask such as NiCr.

Good luck

reply