MEMSnet Home: MEMS-Talk: Re: Thin wafers or SOI wafers
Re: Thin wafers or SOI wafers
1998-01-16
Kai Hiltmann
Re: Thin wafers or SOI wafers
Kai Hiltmann
1998-01-16
> Date:          Tue, 13 Jan 1998 15:44:43 -0800 (PST)
> From:          "Neil (Nick) Talbot" 
> Subject:       Thin wafers or SOI wafers
> My colleges and I are in need of a few thin (150 to 250 microns) wafers.
[...]
> Does anybody have some in stock that we could buy?  Even just
one or two would be great.

Call Sico Meinigen Wafer GmbH
Phone ++49- 3693-71313
Fax ++49- 3693-71315
Mit freundlichen Gruessen, Kai Hiltmann

mailto:[email protected]    http://www.IMIT.Uni-Stuttgart.de
K. Hiltmann
c.o. IMIT
W.-Schickard-Str. 10
D-78052 Villingen-Schwenningen

Tel. ++49-7721-943-236
Fax  ++49-7721-943-210


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Harrick Plasma, Inc.