Re: Surface properties of ITO
2005-02-04
Harald Walter
Re: Surface properties of ITO
Harald Walter
2005-02-04
Hi Paolo,

in the following publication you will find helpful
information:
JOURNAL OF APPLIED PHYSICS VOLUME 84, NUMBER 12, PAGE
6859.
"Indium–tin oxide treatments for single- and
double-layer polymeric light-emitting diodes: The
relation between the anode physical, chemical, and
morphological properties and the device performance"

Harald

> Hi all!
>
> We are trying to modify surface properties of ITO
> (Indium Tin Oxide) using
> oxygen plasma and/or (ozone + UV) treatments.
> But we cannot find data about how long these
> modifications can "survive" in
> air (seconds? minutes? days?).
> Can you please give me any information?
>
> Thank you very much!
>
> Paolo Tassini







___________________________________________________________
Gesendet von Yahoo! Mail - Jetzt mit 250MB Speicher kostenlos - Hier anmelden:
http://mail.yahoo.de

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
MEMStaff Inc.
Process Variations in Microsystems Manufacturing