MEMSnet Home: MEMS-Talk: Metalic vs poly heaters
Metalic vs poly heaters
2005-02-03
Stephen Arnold
2005-02-03
Kirt Williams
2005-02-04
Michael D Martin
Metalic vs poly heaters
Michael D Martin
2005-02-04
Hi Steve,
   You might look into doped silicon carbide or even diamond. You have
one of the world's CVD diamond experts there at NRL, Jim Butler. Of
course you will have to carefully manage loses due to thermal
conductivity.

-Mike