MEMSnet Home: MEMS-Talk: wafer selection for mems
wafer selection for mems
2005-02-11
Ramesh Narayanan
2005-02-11
Pierre Huet
wafer selection for mems
Pierre Huet
2005-02-11
Maybe you should talk to the Si supplier about:
- Crystal defect density (stacking fault, dislocations, etc.); usually
very low in today's materials; maybe also sub-surface polishing damage.
- Oxygen content and chemical state (dissolved, precipitated through
thermal treatment) can affect some mechanical properties like resistance
to fracture. CZ crystal growth process typically introduces tens of ppm
of oxygen in the silicon; FZ process typically has ppb or lower oxygen
in the silicon.
- It is possible that heavily doped Si (~ 0.01 Ohm-cm) has different
mechanical properties than lightly doped (~ 1 Ohm cm) since doping
impurities stress the Si lattice because they do not "fit" as well as Si
atoms in the crystal structure; B and P stress in opposite directions;
Sb stress is low because it fits better than B or P.

Regards,
Pierre x286

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Addison Engineering
Process Variations in Microsystems Manufacturing
MEMS Technology Review