MEMSnet Home: MEMS-Talk: protect thin copper film
protect thin copper film
2005-03-03
Xiaoding wei
2005-03-03
Wilson, Thomas
2005-03-03
Pierre Huet
2005-03-03
David Springer
protect thin copper film
Wilson, Thomas
2005-03-03
Perhaps a 50-A thick Pd coating on top the Cu?