MEMSnet Home: MEMS-Talk: RE: etchant for SiO2 without etching alumina
RE: etchant for SiO2 without etching alumina
1998-02-16
Bai Xu
RE: etchant for SiO2 without etching alumina
Bai Xu
1998-02-16
Try plasma dry etch.

> ----------
> From:         Yagang Li[SMTP:[email protected]]
> Reply To:     Yagang Li;[email protected]
> Sent:         Wednesday, February 11, 1998 6:14 PM
> To:   [email protected]
> Subject:      etchant for SiO2 without etching alumina
>
> Dear colleagues,
>
> My friend gived me this email address because he thought it might
> be a forum site for discussing etching-related issues. Anyway,
> I like to have a goahead.
>
> My problem is to find an etchant for SiO2 which does not substantially
> etch alumina Al2O3. Is somebody there who happens to know the
> formula of this sort of etchant. Your suggestion and help would be
> much appreciated.
>
>
> Cheers.
>
>
> Yagang Li
>
> Department of Materials
> Oxford University
>
> [email protected]
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing