Yuzhu Li
2005-03-14
We have a spinner from "Laurell technology", manually dispence AZ4214.
500rpm,5s--->4000rpm,40s(acceleration=500rpm/s)
After expose with Suss MJB3 alinger, I found PR LW variation of 0.2um
(center wider) from center to edge for 3-inch wafer. At the same time, I
found the PR thickness variation of 0.2um (center thicker).
        Is PR LW variation caused by thickness variation? How to get more
uniform PR thickness, should I use higher spinning speed or higher
acceleration speed?

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
The Branford Group
Process Variations in Microsystems Manufacturing