bosch process
2005-03-15
fabio quaranta
2005-03-15
Burkhard Volland
bosch process
fabio quaranta
2005-03-15
I would like to obtain large and deep hole in Si ( let say 100 um large
300um deep so low aspect ratio). I don't have bosch process fitted in my
ICP system. Someone could tell me if it's possibile to simulate the
process with alternate SF6, CF4 plasmas (adding H2 or Ar if needed)?

Thank you
Ciao
Fabio