MEMSnet Home: MEMS-Talk: how to protect the sidewall of a trench which is 50micron in depth
how to protect the sidewall of a trench which is 50micron in depth
2005-03-29
Brubaker Chad
how to protect the sidewall of a trench which is50micron in depth
2005-03-29
Michael L
2005-03-30
#ZHOU QIAOER#
2005-04-04
Vladimer Michael
how to protect the sidewall of a trench which is 50micron in depth
#ZHOU QIAOER#
2005-03-30
you can try electrodeposited photoresist to protect the sidewall.

Reference:

Carsten Christensen, Peter Kersten, Sascha Henke and Siebe Bouwstra, "Wafer
Through-Hole Interconnections with High Vertical Wiring Densities", IEEE
Transactions on Components, Packaging, and Manufacturing Technology--Part A,
Vol. 19, No. 4, December 1996

hope it helps!

joyce

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Addison Engineering