>Hello,
>We are trying to etch the kapton, but finding difficulties. It is a
>selective etching and we are using photoresist as our mask. We trid etching
>using KOH solution but the etching is very slow. Could any one suggest the
>method of etching the Kapton? The thickness of the Kapton film is 127um.