MEMSnet Home: MEMS-Talk: RE: Transporting SU8 Microstructures.
RE: Transporting SU8 Microstructures.
2005-04-20
Jonathon Gillen
2005-04-25
Michael L
RE: Transporting SU8 Microstructures.
Michael L
2005-04-25
Hi Jonathon,

Let your samples dry out, then try liquid surface tension pick and place. If
you use a pipette, you can place by pressing the rubber baloon to expel the
liquid and your sample with it.

Regards,

Michael

>From: Jonathon Gillen 
>Subject: [mems-talk] RE: Transporting SU8 Microstructures.

>  I am patterning SU8 on top of a thin aluminum layer
>and then etching the aluminum away so that my
>structure is floating in solution.
>
>  Does anyone know of a simple way to pick this
>structure out of the water and transport it? Structure
>size is roughly 5mmx5mmx1um, so it can be easily seen
>with the eyes, but also easily destroyed by mechanical
>stresses.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
University Wafer