Re: Ti etchant not attack glass
2005-04-28
Eric Woods
Re: Ti etchant not attack glass
Eric Woods
2005-04-28
Hydrogen peroxide that is warmed (e.g. 50C) will do that job quite well.

-Eric

> -----Original Message-----
> From: Ming Li [mailto:[email protected]]
> Subject: [mems-talk] Ti etchant not attack glass
>
> Does any body know a Ti etchant and do not attack SiO2?