News
MEMSnet Home: MEMS-Talk: about shadow mask
about shadow mask
2005-04-29
Brijesh Raut
2005-04-29
Kirt Williams
2005-04-29
David Nemeth
2005-04-29
Brubaker Chad
about shadow mask
David Nemeth
2005-04-29
One option is to use a laser cut stainless steel foil, of the type used for
stencil solder paste on PCB boards.  One such company is :
http://www.stencilsunlimited.com/
There are others.

David Nemeth
Senior Engineer
Sophia Wireless, Inc.

-----Original Message-----
From: Brijesh Raut
Subject: [mems-talk] about shadow mask

Can anyone tell me the names of the companies, who fabricate or produce
shadow mask for metal deposition.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics