Hi Yanli,

It is generally under tensile stress - i.e. bending away from the substrate.

Michael

>From: "yanli Wang" 
>Subject: [mems-talk] Initial Stress of SU-8
>I would like to know the initial stress of SU-8. Is the SU-8 compressive
>stress or tensile stress?