MEMSnet Home: MEMS-Talk: Re: Photoresist for Silicon DRIE
Re: Photoresist for Silicon DRIE
2005-05-20
Stephen Arnold
Re: Photoresist for Silicon DRIE
Stephen Arnold
2005-05-20
Stephan --

Most often, SiO2 is used as the etch mask for DRIE. Nitride would work
as well.

Stephen Arnold
The George Washington University
School of Engineering and Applied Science
reply