PDMS adhesion
2005-05-30
Yi Zhao
2005-05-31
Alik Widge
PDMS bonding to glass
2005-06-01
Kamat Mahesh Keshav
2005-06-01
Lee Pang
2005-06-01
Lee Pang
2005-06-01
Xin Liu
PDMS adhesion
Xin Liu
2005-06-01
Hi,
I don't know exactly the processes you described. But I know that PDMS will
swell in acetone. It might caused by the mechanical strain between PDMS and
your substrats.

Xin Liu(Mr.)
Dalian Institute of Chemical Physics,
Chinese Academy of Sciences

-----Original Message-----
From: Yi Zhao [mailto:[email protected]]
Subject: [mems-talk] PDMS adhesion

I found in my experiments that acetone is good to release bonded PDMS
surfaces. But I do not how it works. Does anyone have experience or can
provide some references what exactly acetone does to the interfacial
adhesion of PDMS?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
University Wafer
Nano-Master, Inc.