We use a splay pattern to determine the exact orientation
of wafers for anisotropic etching.  Unfortunately we have
"dropped" the mask and have had to resort back to x-ray
diffraction.  Does anyone know of a commercial source
for these splay patterns?

best regards
mark

Mark W. Lund, PhD
Director             >> Soft X-ray Web page http://www.moxtek.com<<
MOXTEK, Inc.
452 West 1260 North
Orem UT 84057       801-225-0930        FAX 801-221-1121
[email protected]

"The state is good at simple tasks, like killing people and seizing their
wealth.  It has far more trouble reaching inside individuals and making them
good." Doug Bandow


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics