Dear colleagues,
has someone expriences with the "Ultradel 9120d" polymide by Amoco for
making monomode waveguides in the near IR region? What about the
adhesion to a fused silica surface?Any help would -again- be
appreciated!
Yours regina


--
________________________________________________________________________

Dipl.-Ing. Regina Grote                  e-mail:[email protected],

AG Integrierte Optoelektronik            tel:   +49-(0)631-205-4149
Universitaet Kaiserslautern              fax:   +49-(0)631-205-4147

Erwin-Schroedinger-Str 46, 67653 Kaiserslautern, Germany


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics
University Wafer