MEMSnet Home: MEMS-Talk: PDMS Sticking to PDMS
PDMS Sticking to PDMS
2005-06-12
Terry Barchfeld
2005-06-13
ssood
2005-06-13
Dwayne Dunaway
2005-06-13
Lee Pang
PDMS Sticking to PDMS
ssood
2005-06-13
Hey Terry,

what are you mixing the PDMS with.? You can mix PDMS with hexane (95%
n-hexane) in different ratios, the two mixtures will adhere to each other. If
you send me an email explaing your exact thing, I might be able to give
more input.

Thanks
Sumant Sood
Belford Research