A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: high melting-point wax
high melting-point wax
2005-06-15
Mac Daily
2005-06-15
Minghai Li
high melting-point wax
Mac Daily
2005-06-15
Zhou,

Does it have to be wax?  PMMA has a Tg of 105C and works well for sticking
wafers together.

Mac
--
Madison "Mac" Daily
New Business Development Manager
Specialty Materials Division
Brewer Science, Inc.
Telephone: (573) 364-0300
Fax: (573) 458-4372


> From: "D. Zhou" 
> Subject: [mems-talk] high melting-point wax
>
> Does anyone know where I can get some high melting-point wax which can be
> used to stick the chip at a temperature of about 80 degrees? I tried black
> wax but it melt at 80 degrees. Many thanks.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing