Anyone has experience with the e-beam evaporation of Pyrex glass? We have
tried to evaporate Pyrex glass by e-beam and experienced flaks on the
surface besides good thin film deposition. Any input would be appreciated.

Decai
************************************************
Decai Sun, Ph. D
Electronic Materials Lab
Xerox Palo Alto Research Center
Palo Alto, CA 94304
phone:650-812-4169, fax:650-812-4105
email:[email protected]
************************************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMS Technology Review
MEMStaff Inc.