MEMSnet Home: MEMS-Talk: Gold undercut
Gold undercut
2005-06-17
kris
2005-06-18
Lou Chomas
Appropriate microwave frequency for heating nanoparticle under fluid flow in a cylindrical resonantor
2005-06-20
wahid YEMI.
Gold undercut
Lou Chomas
2005-06-18
Kris,
      Almost all Au etches will undercut the mask to some exent.  Is this
what you mean by undercut?  You could possibly improve this by using a hard
mask such as SiO2.  It may be that the resist is not adhereing too well to
your Au.

-Lou

>From: kris 
>Subject: [mems-talk] Gold undercut
>Date: Thu, 16 Jun 2005 21:37:26 -0700 (PDT)
>
>I was wondering if KI+I2+H2O undercuts gold??
>
>Is there any AU etchant that does`nt undercuts AU.
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Addison Engineering