A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: About the Piranha cleaning
About the Piranha cleaning
2005-07-14
Zhiwei Zou
2005-07-14
Sumant Sood
2005-07-14
Hongjun-ECE
2005-07-15
Zhiwei Zou
2005-07-15
Brent Garber
2005-07-15
Jesse D Fowler
2005-07-15
Sumant Sood
2005-07-15
Barry Isenor
2005-07-15
Virginia Abranches de Sousa R. Soares
2005-07-15
Shile
2005-07-15
Gary
About the Piranha cleaning
Barry Isenor
2005-07-15
Always add 1 part H2O2 to 3 parts H2SO4.

Barry Isenor
System Integration
Electrical and Computer Engineering
University of Calgary


-----Original Message-----
From: Hongjun-ECE [mailto:[email protected]]
Subject: RE: [mems-talk] About the Piranha cleaning

Belford,

Please confirm that it is H2So4 added to H2O2, instead of H2O2 added to
H2So4, which might be dangerous.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing