MEMSnet Home: MEMS-Talk: Re: Black spots on PDMS!!!
Black spots on PDMS!!!
2005-07-19
Vishwanath Somashekar
Re: Black spots on PDMS!!!
2005-07-22
Marc Hennemeyer
PDMS bonds to silicion wafer?
2005-07-27
[email protected]
2005-07-28
Cheng Ming Lin
Re: Black spots on PDMS!!!
Marc Hennemeyer
2005-07-22
Vishwanath Somashekar wrote:
> b) NaOH (0.3mol/litre) mixed with a littel DI water and then Ethanol
snip...
> On the NaOH side of the channel, after
> running the solutions for about an hour or so, I see black deposits on
> the PDMS.

I am not a chemist, but to me it sounds, as if the NaOH reacts with the PDMS and
sets
carbon free. Check the chemical stability.

Marc

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMStaff Inc.