MEMSnet Home: MEMS-Talk: SU-8 UV degradation
SU-8 UV degradation
2005-08-02
Michael L
2005-08-02
[email protected]
2005-08-04
Michael L
SU-8 UV degradation
Michael L
2005-08-04
I was thinking more about prolonged, high intensity UV exposure. Ambient
doses are unlikely to have an effect.

Michael

>Greetings,
>I don't believe there is a UV problem.
>We developed finger print ID devices that had a final coating of SU8 ,we
>found no degradation during testing to my knowledge.
>Regards
>walter
>www.elume.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
Process Variations in Microsystems Manufacturing
University Wafer