Dear colleague,

   Recently I want to spin-coat copolymer P(VDF-TrFE) thin films on the
 Al-coated glass substrate, but the adhesion between coplymer and
Al-coating is not good, and the whole films is not uniform with many
holes. how to improve the adhesion and form the uniform copolymer thin
films by the spin-coating method.Please give me advice if you have
exprience in this field.Many thanks.

 Regards
 J.J.Li
 Research Institute of Electronics
 Shizuoka University
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
The Branford Group
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing