MEMSnet Home: MEMS-Talk: Etching Si (110) wafer without attacking Metal pads
Etching Si (110) wafer without attacking Metal pads
2005-11-21
Tao
2005-11-22
Simon Garcia
Etching Si (110) wafer without attacking Metal pads
Tao
2005-11-21
Dear All,
   I want to etch (110) Si wafer (200~300um thick) to release my
cantilever. However the Al pads for electric contact will be etched too.
So I am wondering if there are other metals that have a high resistance
to KOH? The important thing is that the wafer will be etched for about
2~3 hours in KOH (20% ~ 60%, not decided yet) at 80 degree C.
   Thanks a lot!

HTao
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing