MEMSnet Home: MEMS-Talk: SU-8 mold for Au electroplating : SU-8 is not developed well
SU-8 mold for Au electroplating : SU-8 is not developed well
2005-12-19
aeroalto
SU-8 mold for Au electroplating : SU-8 is not developedwell
2005-12-19
Richard H. Morrison
2005-12-20
Lung-hao Hu
SU-8 mold for Au electroplating : SU-8 is not developed well
Lung-hao Hu
2005-12-20
Try to use Remover PG with Ultrasound and at 60 C.
Or coating Omnicoat before SU-8 coating......

Lung-hao Hu

Graduate Student

Dept.of Mechanical Engineering
Univ.of Colorado Boulder
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
MEMS Technology Review
Nano-Master, Inc.