MEMSnet Home: MEMS-Talk: <None>
<None>
1998-06-10
Jim Intrater -- FR
Jim Intrater -- FR
1998-06-10
I need to find a company (preferably, but not necessarily, on the west
coast) that can apply a resist layer to a 2.5" square of aluminum oxide
and image some 1 mil (25 microns) wide, free-standing bars at at least 1
to 2 mils (25 to 50 microns) tall. Do you have any suggestions?


 Jim Intrater
 Oryx Technology Corp.


reply