MEMSnet Home: MEMS-Talk: etching of Pt
etching of Pt
1998-06-10
Mounir Ennabli
etching of Pt
Mounir Ennabli
1998-06-10
Hi,
dear members
I am investigating the etching rate of platinum (Pt) in aqua regia. I
use a modified recipe of aqua regia: 8vol.H2O,7vol.HCl,1vol.HNO3 at 85 C
degrees. Does any body have some
informations about this process? I know that the rate should be high,but
'how high'?
Thanks on  forehand.
Mounir Ennabli.

------------------------------------------
Mounir Ennabli, Transducer group
Mikroelektronik Center
Technical University of Denmark
Room 154, building 345E, 2800 Lyngby
Phone(o): +45 4525 5734
Phone(h): +45 4587 3535-1283
Fax:     +45 4588 7762
e-mail: [email protected]
http://www.dtu.dk/mic/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Nano-Master, Inc.
MEMS Technology Review