hi all,
   We have a few silicon wafers with teflon coating on it. We would like to
etch few holes into silicon (as we already did few holes onto the teflon).
we need depths of 400nm in these silicon wafers. can anyone suggest a few
isotropic etchants and etch rates for this silicon with teflon coating on
it.

thanks in advance,
Jeeva