Polyimide on silicon nitride
2006-02-03
Mehmet Unlu
2006-02-04
[email protected]
Polyimide on silicon nitride
[email protected]
2006-02-04
Polyimides are problematic depending on the formulation of the Polyimide.
Some contain fillers like carbon like materials that only seem to etch in the
presence of fluorine. It also helps to keep the substrate cooled and use a
powerful ICP source to generate the density of oxygen radicals used to etch the
imide. We use a system that has both a powerful ICP and rie for directionality
in
removing polyimides. During the etch phase we also include 1-3% of the total
flow of CF4 or CHF3 to remove any filler materials that can slow or stop the
etch. Since you are trying to free an aluminum feature you should be able to
release it by removing the polyimide from under the feature up to a point. Bob
Henderson
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.