Deposition of nitride on metal
2006-02-05
Rakesh Poddar
2006-02-05
PRAMOD GUPTA
Deposition of nitride on metal
PRAMOD GUPTA
2006-02-05
Rakesh

  What type of nitride (SiN or TiN or TaN or AlN etc) do you want to deposit on
Al or Cr layers?

Rakesh Poddar  wrote:
  Hi,

I want to electrically insulate my metal patterns (Al, Cr) by depositing a
nitride layer...Is it possible to deposit LPCVD or PECVD nitride on the metal
layer particuarly Al and Cr.. If anybody has prior experience on this kind of
process, please comment...
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing