Dear all,

I would like to plate electoless nickel onto
Borofloat 33 glass from Schott, alternatively
AF45.

First trials showed very bad adhesion.  I think
the problem is the very low surface roughness of
the glass.

I would be very happy if someone could help me
with some guidelines on how to get good adhesion.

Thanks,
Jurgen
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer
The Branford Group